TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Reuven ROKAH <[log in to unmask]>
Date:
Mon, 20 Oct 2003 09:01:35 +0300
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "S.R. Madhuchandra" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (71 lines)
You may have internal stresses inside the layers because of poor design or
press thermal cooling cycle or the peelable is too thick that expand /
shrink during the thermal curing.

Best  Regards

ROKAH Reuven




                      "S.R.
                      Madhuchandra"              To:      [log in to unmask]
                      <s.r.madhuchandra@         cc:
                      IN.ATS.NET>                Subject: [TN] Warpage after PLSM
                      Sent by: TechNet
                      <[log in to unmask]>


                      20/10/2003 09:12
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to "S.R.
                      Madhuchandra"





fellow technetters

In some of the part numbers, we are facing a strange phenomenon

The boards will be flat till the process of PLSM(peelable solder mask)
but after the PLSM, there will be severe warpage & wobbling

In PLSM, we are doing both UV & thermal curing

Can some one throw some light on this

Thanks in advance
Madhu


Scan by AT&S virus protection

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2