hi,
i think the issue here is one of using a diode that has a terminal finish that is best suited to hybrid wire bonding, conductive adhesive attach, etc.
tin lead solders wash off the gold which is all there is on these parts. last i heard, soldering to ceramic is pretty difficult.
phil
-----Original Message-----
From: Dave Chapman [mailto:[log in to unmask]]
Sent: Thursday, October 09, 2003 8:47 AM
To: [log in to unmask]
Subject: Re: [TN] Flip Chip Diode 0205
Spec on component says use solder which does not scavenge gold such as
Indalloy #2, or conductive epoxy or low temp solder preform.
Also says cannot withstand 200 C for more than 10 seconds.
Dave C.
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Thursday, October 09, 2003 10:27 AM
To: [log in to unmask]
Subject: Re: [TN] Flip Chip Diode 0205
Hi Dave,
You are not clear as to what "cannot go through Sn-Pb due to embrittlement"
means. Preforms, as well as Sipad are also Sn-Pb.
I have no experience with conductive epoxies, but know that they are not as
good as solder from a reliability perspective.
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|