text/plain (33 lines)
I have now learned that /22 (and for that matter /23) are no longer
readily available.  The /21 is too low of a temperature.  I am being
steered to /24, but I need to know whether my original GBN qualification
will still be valid.

Any words of wisdom?  Thanks!

============================================

We have a qualified product based on using GBN board material per
MIL-P-13949.   Upon investigating IPC-4101 I notice that /22 is NEMA
G-11 - GB (no reference to 13949) and that /21 is MIL-S-13949/04 -
GF/GFN/GFK.  The issue I have is that GB has a much higher temperature
range than GF.

My question is what is the current material spec that corresponds to
the original 13949 GBN?

Thank you for your assistance.

Regards,
Jim

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2