Steve: The real advantage of the silicone over the urethane is it's
temperature resistance(200C) and stability of electrical properties at
elevated temperatures. If you don't need this use the urethane.


Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076



-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Thursday, September 04, 2003 12:35 PM
To: [log in to unmask]
Subject: [TN] Silicone conformal coating


Hi All!

I know when you look up properties for Silicone conformal coating, it
usually states that it has good moisture resistance, but is it really that
good?

I've heard that it is somewhat permeable to moisture, that if you were
worried about moisture, and the assembly were going to see the outside
environment, you would be better off with an acrylic, or urethane coating.

Any thoughts?

Thanks!

-Steve Gregory- ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2