Select your PWB storage location carefully-- one assembler (nameless) stored
their silver-bearing PWBs in a location that guaranteed tarnishing-- right
next to the company cafeteria. Yes, they did work 3 shifts/day and yes they did
feature eggs on the breakfast menu..... 'nuff said.
Bill Kenyon
Global Centre Consulting
P.O. Box 553, Montchanin, DE 19710 USA
Tel: 302.652.4272 Fax: 302.652.5701 Cell: 302.377.4272
email: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------