General adhesive bonding (i.e. aluminum to fiberglass, etc.) in a fairly
clean factory environment.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: joyce [SMTP:[log in to unmask]]
Sent: Thursday, September 18, 2003 7:36 AM
To: [log in to unmask]
Subject: Re: [TN] contamination-free gloves
Jim,
What bonding? Adhesive bonding or wire bonding? In what class of
cleanroom? Handling PWB? Ceramic? Chip?
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
>Sent: Thursday, September 18, 2003 2:17 AM
>To: [log in to unmask]
>Subject: Re: [TN] contamination-free gloves
>
>
>Whichever gloves you choose, I suggest you do an ionic
>contamination test on them. The residues from latex coagulants
>may be ionic, as may flexibilisers and anti-static agents.
>Also, moulded gloves may have either fluorinated or silicone
>release agents on them. Latex often has a fine powdering of
>talc. Careful choice required.
>
>Brian
>
>Marsico, James wrote:
>> Hello Technet:
>> I'm looking for suggestions for contamination-free (silicone,
etc.)
>> gloves to be worn by operators performing a bonding operation.
I'd
>> prefer something like latex or nitrile rather than cotton, if
such a
>> thing exists.
>>
>> Thanks in advance,
>>
>> Jim Marsico
>> Senior Engineer
>> Production Engineering
>> EDO Electronics Systems Group
>> [log in to unmask] <mailto:[log in to unmask]>
>> 631-595-5879
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using
>LISTSERV 1.8e To
>> unsubscribe, send a message to [log in to unmask] with
>following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To
>temporarily halt
>> or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all
the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the
>> archives of previous posts at:
>http://listserv.ipc.org/archives Please
>> visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>> -----------------------------------------------------
>>
>>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV
>1.8e To unsubscribe, send a message to [log in to unmask] with
>following text in the BODY (NOT the subject field): SIGNOFF
>Technet To temporarily halt or (re-start) delivery of Technet
>send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail
>to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|