Charles,
We saw the same problem with the Pace, we solder a variety of
high temp alloys and ended up with the Hakko FM202. Much better results
and special tips available for soldering HMP and gold....
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charles Caswell
Sent: Wednesday, September 17, 2003 6:49 AM
To: [log in to unmask]
Subject: Re: [TN] Pace soldering irons
We had one of these to checkout last Fall. We found that the temp.
recovery was slow compared to our Metcal. For most jobs the iron worked
fine but when we tried to solder anything heavy we had problems.
-----Original Message-----
From: Diamond, Pat [mailto:[log in to unmask]]
Sent: Wednesday, September 17, 2003 2:32 AM
To: [log in to unmask]
Subject: [TN] Pace soldering irons
Hi all,
We have just purchased some of the new Pace Tempwise soldering irons
which are microprocessor controlled, we are having a few teething
problems with stability when checking the tip temperature. Has anyone
out there had any experience with this problem?
We are using a Hakko 191 thermometer to check the tip temperature.
Thanks,
Pat
************************************************************************
****
***************
The information transmitted is intended only for the person or entity to
which it is addressed and may contain confidential and/or privileged
material.
Any review, retransmission, dissemination or other use of, or taking of
any action in reliance upon, this information by persons or entities
other than the intended recipient is prohibited. If you received this in
error, please contact the sender and delete the material from any
computer.
************************************************************************
****
***************
Pat Diamond
Senior manufacturing Engineer
Weston Aerospace Tel: +44 (0)1252 868194
124 Victoria Road Fax: +44 (0)1252 370298
Farnborough, Hampshire, GU14 7PW Web www.westonaero.com>
England Email mailto:[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|