Hi Carl,
These boards have not been processed thru the screen printer. the problem
was initially found from assembled boards, so I began eliminating various
possibilities by running the raw board through the oven and found that the
solder balls still existed. I have seen the misprint issue you mention,
where the boards were not thoroughly cleaned afterwards and solder balls
developed the way that you describe, but this was not the problem in this
instance. Thanks for the input, though.
Thank you,
Paul Black
Manufacturing Engineer
Kronos
-----Original Message-----
From: Carlr Ray [mailto:[log in to unmask]]
Sent: Thursday, September 25, 2003 6:55 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Balls
Paul,
Just to make sure we are talking about the same process here, these
boards have not been processed thought the screen printer, correct? If
so I have seen where improper cleaning practices from mis prints cause
trapped solder spheres and result in solder balls. Most of the trapped
paste is located around the vias and PTH barrels. Some can become
trapped in corners of SMDP (Solder masked defined pads). Just a question
to make sure nothing from the process was inducing the solder balls.
>>> [log in to unmask] 9/24/2003 6:57:24 AM >>>
Hi TechNet Gurus,
Has anyone experienced solder balls resulting from the board
fabrication
process? We have been getting them from our offshore supplier for a
few
months now and have had to add a wash step to our no-clean process. We
know
that it's fro the board because we have run bare boards through the
reflow
oven using the normal reflow recipe from that board and we are seeing
25-60
random solder balls on our 9" x 7", 8 layer, .062", HASL FR4 board.
We
believe the problem is caused by uncured solder mask that erupts when
exposed to reflow temperatures but have been unsuccessful trying to
eliminate the problem. We have tried baking the board @ 320 F for
anywhere
from 1.5 - 6 hours. This has reduced the number of solder balls to
maybe a
dozen or less. Anyone have a suggestion?
Thank you,
Paul Black
Manufacturing Engineer
Kronos
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|