Peter,
As to processing options, I see two paths to choose from if your goal is to
stick with soldering. As was said already, silver epoxies have several
undesirable qualities when mixed with HASL and "rigid" substrates so I too
am discounting them as a preferred option.
I'm not clear as to whether the LEDs are the only part on the board in
question so adjust to fit.
1) Solder pastes exist that are designed to withstand the temperature
cycling typical of iron and laser heating without explosive vaporization
issues. They can be dispensed or printed depending upon the processing
options available to you. Flame, as a heat source, can ignite solvent
vapors and rosin in the flux so I, personally, would stay away from them
unless you could avoid said ignition.
2) You could also try pre-pasting the pads, along with the rest of your
standard board assembly (if there is any), and later using a tacky flux for
component attach and reflow. The likelihood of solder balls is
exceptionally low regardless of heating method (as there are none to wash
free with the flux).
Depending upon production quantities and accuracy requirements, such systems
as tabletop automation, with integrated dispensing and heating, might be a
more cost effective solution than manual alternatives. Only a cost
comparison will answer that question.
John Vivari
Technical Service Engineer
Solder Paste Operations
EFD Inc.
[log in to unmask]
www.efdsolder.com
Ph: 401-333-3800
Fx: 401-333-4954
-----Original Message-----
From: Peter Swanson [mailto:[log in to unmask]]
Sent: Friday, September 12, 2003 4:57 AM
To: [log in to unmask]
Subject: [TN] LED Soldering Query
We have a customer who is looking at assembling some surface mount LEDs to a
FR-4 board. We are told that the parts will not stand conventional reflow
temperatures (they themselves are made with a LMP solder, and the lens is
temperature sensitive). At this stage, I don't know much more detail.
The query is whether he could print conventional paste, place the devices
and then reflow each joint individually, by using a robot. But a soldering
iron applied the paste will cause spitting, solder balls, etc.
Perhaps a thermode could be applied to the joint and a temperature ramp up
applied, which will safely reflow the paste, if such a thing exists and can
be mounted to a robot.
I would be interested in general thoughts on how to process these parts.
Maybe not even solder...
TIA,
Peter
--
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material,
consumable and equipment solutions to high technology
assembly industries, with the highest levels of technical
support and customer service.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|