TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Misner, Bruce" <[log in to unmask]>
Date:
Mon, 8 Sep 2003 17:31:00 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; format=flowed
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (92 lines)
Of course silicone will repel liquid water, but we are talking here of
water in a gaseous phase and my experience is that it passes small
molecules, such as water, like a sieve. In the former case, it is a
question of the high surface tension of water, but single molecules, ata
a time, have no surface, therefore no surface tension.

Brian

Misner, Bruce wrote:
> Brian,
>
> This diaphram experiment does not take into account the surface
> wettability of Silicone which is supposed to be one of its major
> protective features (according to Dow) which precludes surface droplets
> from forming. Comments?
>
> Thanks,
> Bruce Misner
>
>     -----Original Message-----
>     From: Steve Gregory [mailto:[log in to unmask]]
>     Sent: Monday, September 08, 2003 8:54 AM
>     To: [log in to unmask]
>     Subject: Re: [TN] Silicone conformal coating
>
>     In a message dated 09/05/2003 2:03:30 AM Central Daylight Time,
>     [log in to unmask] writes:
>
>
>>     I thought I had reported the details of this in
>>     my book, but could not find them today. Must have been somewhere else.
>
>
>
>     Hi Brian!
>
>     It is in your book, on page 329, at the bottom of the section where
>     you talk about Silicone Elastomers.
>
>     In your book you state that you made a diaphram of silicone that was
>     5mm thick, and 100mm in diameter. On one side the air was held at 40
>     degrees C., and 95% RH, the other side at 5% RH. There was 1g of
>     water vapor per day allowed to pass through the silicone diaphram.
>     You stated that is 40 times worse than epoxies, and 20 times worse
>     than polyurethanes.
>
>     Do you have any idea about arcylics?
>
>     Regards,
>
>     -Steve Gregory-
>     ---------------------------------------------------
>     Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>     To unsubscribe, send a message to [log in to unmask] with following
>     text in the BODY (NOT the subject field): SIGNOFF Technet
>     To temporarily halt or (re-start) delivery of Technet send e-mail to
>     [log in to unmask]: SET Technet NOMAIL or (MAIL)
>     To receive ONE mailing per day of all the posts: send e-mail to
>     [log in to unmask]: SET Technet Digest
>     Search the archives of previous posts at:
>     http://listserv.ipc.org/archives
>     Please visit IPC web site
>     http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>     information, or contact Keach Sasamori at [log in to unmask] or
>     847-509-9700 ext.5315
>     -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2