Hi Marie,
To my opinion Brian is right, but also I believe he may forget about
the fact that you need to be competitive. When you use a material that's
designed to leave only harmless residues, you should be relatively safe.
If your products need to have high reliability, or if they need to
operate in a humid atmosphere I still wouldn't leave the material on the
board, but for other products it seems to me it could very well be
acceptable. I mean why would you strive for a cleanliness level that
guarantees 30 years lifetime if the product will be thrown away in 3
years anyway ?
Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 09/04/03 12:54pm >>>
No way should anything, designed to be temporary, become permanent.
Even
residues, after peeling, can be dangerous unless meticulously removed.
Donkey's years ago, I took a 10 cm x 10 cm board which had been
meticulously cleaned to near-zero ionic contamination. I then coated
it
entirely on one side with a layer of peelable mask (and I tried it
with
about 8 different makes). I allowed the mask to dry 24 hours, to be
sure
that all volatiles had gone. I then carefully peeled off every visible
trace of the mask and done ionic contamination tests on each board. In
EVERY case, the ionic contamination had risen by some degree, mostly
to
a quite dangerous level (exact figures lost in the mists of time). If
the invisible residues will do this, just imagine what visible
residues
will do.
My answer is a categorical NO. In fact, I would go farther: peelable
masks should never be used in a "no-clean" situation (or after
cleaning)
where quality and reliability are criteria to be respected (this will,
no doubt, hurt some, but it is my belief).
Brian
Dobbs, Marie wrote:
> I am looking for some feedback. We use Techform Liquid solder mask
> (peel able) to cover PTH on our PCA's.
> We also use this Mask as a "Tacking" mechanism to hold Loose Loaded
> (unsecured/not bent) components on the top side of the board. After
the
> mask dries, we take it off the board. This is a Non-Value added
> activity that I would like to eliminate. I want to leave the dried
> masking on the board.
> My question is. Can I leave it on the board? Will it affect the
long
> term function of the board? Do any of you use this, or do this?
Any
> input is appreciated.
> Thanks
> Marie
>
>
> Marie A. Dobbs
> Training and Development Specialist
> Tyco Safety Products
> 100 Technology Drive
> Westminster, MA 01473
> Phone: 1-978-731-6827
> Fax: 1-978-731-6950
> email: [log in to unmask]
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
> To unsubscribe, send a message to [log in to unmask] with following
text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|