TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Mon, 29 Sep 2003 09:40:44 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Smith, Russell (US LA)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Smith, Russell (US LA)" <[log in to unmask]>
Parts/Attachments:
text/plain (120 lines)
Just saw this message after I wrote the other and answer to the other one. with the 150F temperature you really don't need the rest if you don't use a lot of low boiling solvent to thin it.

 52 is a 100% epoxy system, not a blend like 77. 52 uses a salt type hardener( actually a combination of 2 cationic acid hardeners. the melting point for one of these is 49C the other 86.4C
( 120F and 188F respectively) , so at 125F you would get some curing of the material, however it would not reach the point of sure it could at a temp above 188F. 

-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Monday, September 29, 2003 7:01 AM
To: [log in to unmask]
Subject: Re: [TN] Probimer 77 soldermask


Thanks again. One last question. My customers procedure was written for Probmer 52 and calls for 1Hr room temp. followed by 4 Hr. at 150 deg.F. My first sample was still soft after this and could be rubbed off with a soft cloth and alcohol.
 What would be your recommended cure time at 150deg.F? I don't think they will allow a higher temp.
Charles Caswell

-----Original Message-----
From: Smith, Russell (US LA) [mailto:[log in to unmask]]
Sent: Friday, September 26, 2003 3:13 PM
To: [log in to unmask]
Subject: Re: [TN] Probimer 77 soldermask


the ratio is 82 parts 1040 to 18 parts 1050, The thinner you can use will depend on how long you want to have brush ability , before the solvent evaporates. The good Solvent is PMA, but you might want to use some MEK , if you need it to air dry fast. Don't use acetone, it usually has to much water in it and it will make a mess. 

Russell Smith

-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Friday, September 26, 2003 12:29 PM
To: [log in to unmask]
Subject: Re: [TN] Probimer 77 soldermask


Thank you. I have the info now. I am using 1040 with hardener 1050. This is for touch up on a board that the original mask peeled from several areas. Since I will be applying it with a brush is there a thinner I can use?

-----Original Message-----
From: Smith, Russell (US LA) [mailto:[log in to unmask]]
Sent: Friday, September 26, 2003 1:51 PM
To: [log in to unmask]
Subject: Re: [TN] Probimer 77 soldermask


Charles, 
If you could give me the product numbers of the hardener and resin you are using , ( they should be like 1040, 1070 , etc,)  I can give you the precise ratios. 
Thank you 
Russell Smith
Huntsman Advanced Materials 

-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Friday, September 26, 2003 7:57 AM
To: [log in to unmask]
Subject: [TN] Probimer 77 soldermask


Anybody know the mix ratio for this?
Charles Caswell
The Big Kahuna

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2