TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Date:
Fri, 19 Sep 2003 10:13:37 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Content-Type:
text/plain; charset="iso-8859-1"
In-Reply-To:
Organization:
EXFO-TO
MIME-Version:
1.0
Parts/Attachments:
text/plain (54 lines)
That is very strange.  Normally, the mounding compound MUST pass the
ionic extraction test for each lot.  Any extractable ionics normally get
caught, particularly, when you qualify a new formulation.   Something is
not add-up.... By knowing Sumitomo, they are very commited to quality.
It shouldn't happen.  But as you mentioned, it did happen, This is very
serious.... Normally you use one moulding compound for many parts...Not
something you want to think about on Friday... ;-(

jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven
>Sent: Friday, September 19, 2003 9:55 AM
>To: [log in to unmask]
>Subject: [TN] Potential Problems with Mold Compound
>
>
>Had anyone seen this yet.  It just came to my attention this morning.
>
><http://www.maxim-ic.com/TechSupport/QA/Reliability/SumitomoNote.pdf>
>
>I wonder just how much (other) product has been manufactured
>with this particular mold compound, and how many
>under-explained failures it will generate?
>
>
>Steven Creswick - Gentex Corporation
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV
>1.8e To unsubscribe, send a message to [log in to unmask] with
>following text in the BODY (NOT the subject field): SIGNOFF
>Technet To temporarily halt or (re-start) delivery of Technet
>send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail
>to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2