Hi Neighbor,
Dendrite and related Electrochemical Migration is supported by residual
contamination, moisture and bias. Have you tried an extraction cleanliness
method/test like IC or HPLC to determine cleanliness? (Not Ionic
Conductivity)
Best regards,
Mel Parrish
Madison, AL 35758
256 705 5530
256 461 9566 Fax
[log in to unmask]
www.solderingtech.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Carlr Ray
Sent: Monday, August 11, 2003 1:05 PM
To: [log in to unmask]
Subject: [TN] Dendritic growth tests
Hello All,
I have received components from a certain vender in the past and over
a period of time the parts experience rapid dendritic growth. We have
tested the parts per the following specs, but I was wondering if there
were any other tests that could help us determine this issue sooner?
Specs: Telcordia GR-78
Component Type: QFP 44 pin
Carl Ray
Sr. Manufacturing Engineer
Huntsville, AL 35807
Phone: 256-882-4800 ext. 8845
Cell: 256-990-1990
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|