Agreed, Immersion Silver was a drop in replacement both at reflow and wave.
Silver was lower cost or same as HASL. Only caution, the joints do look
different than HASL boards so education rather than rejection is the word of
the day.
As with all alternate finish boards handling is important, hands off the
board, slip sheets needed on only the top and bottom boards since the
finish is actually below the surface of the solder mask so no big risk of
scratching) in vacuum sealed bags, remove from packaging just before
processing, don't let sit on the shelf unless fully processed, don't wait
3-4 weeks to run through the wave after SMT because you may see tarnish,
although solderability is still good, statistically the sooner processed the
better.
White Tin we had to go to higher temp profile and watch every step.
Congratulations on going to Lead Free PCB's
Dave Chapman
-----Original Message-----
From: Bill DeCray [mailto:[log in to unmask]]
Sent: Thursday, August 28, 2003 11:34 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Silver vs. White Tin
Immersion silver would be the best choice
Highest Regards
William W. DeCray III
Sales Engineering Manager
Waytec Electronics Corp.
Phone: (434) 237-6391 Ext 115
Fax: (434) 237-1324
Cell: (434) 851-6115
E-mail [log in to unmask]
Website www.waytec.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, August 28, 2003 11:31 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver vs. White Tin
Hi All!
Got a customer that's calling out on the fab drawing, either Immersion
Silver
or White Tin for a board finish.
Me, not having great deal of experience with either one (yet), am
wondering
if I had to choose, which one would I choose?
Have any of you worked with both, and have a preference of one over the
other? Why?
As always, thanks in advance!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|