TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Frank L Norman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 11 Aug 2003 14:48:10 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (114 lines)
All,
While you are all on the subject of ENIG plating soldering issues. Take a
look at these examples of solder pads that are not salvageable. This
failure took place in the wave solder process. Currently we are waiting
failure analysis results.

Hype link to pictures as follows...
Click on thumbnails to see larger views.
http://www.ripus.com/images/pwa/index.htm

Regards,
Frank Norman
Manufacturing Support Engineer
Raytheon, Space and Airborne Systems (SAS)
(805)879-2745
[log in to unmask]





Dave Hillman <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/11/03 12:30 PM
Please respond to "TechNet E-Mail Forum."; Please respond to ddhillma


        To: [log in to unmask]
        cc:
        Subject: Re: [TN] Black pad


Hi Werner! We have tried to use our ROSA system to electrochemically
reduce
the degraded nickel surfaces with no success (nickel oxide/corroded nickel
is tough stuff!). I have not heard of anyone being able to restore a
"black
pad" surface successfully without having collateral damage to adjacent
regions of the printed wiring assembly.

Hey Rudy S. - is there a chemical treatment potential/possibility?

Dave Hillman
Rockwell Collins
[log in to unmask]



                      Werner Engelmaier
                      <[log in to unmask] To:
[log in to unmask]
                      OM> cc:
                      Sent by: TechNet Subject: [TN] Black pad
                      <TechNet@listserv
                      .ipc.org>


                      08/11/2003 02:09
                      PM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      Engelmaier






Hi All,
Are there any successful rework procedures for 'black pad'?

Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2