We're using standard NC solder 63/37... and 65C flux...
The wetting's just not happening on the board side... we've done these for
years without this problem... it's kind of looking like solder fractures.
Soldering irons: Hakko 936 ESD with 1.2 tips... temps: 750F
Our Cleaning capabilities? ... Ultrasonic/deionized H20... we also have some
Bronson mix...
We have not washed these, but I wanted to throw this out to you all to see
if this may be pointing to some other problem... Any assistance is
appreciated...
John Grabski III
Badger Technologies Inc.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------