TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Grabski III, John R." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 7 Aug 2003 15:48:26 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (102 lines)
hmmm...

What catalog carries these? Or are they no longer manufactured?

- John Grabski III
Badger Technologies, Inc.


-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: Thursday, August 07, 2003 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] marking screws at torque step


Whoa! Wish those had been available when I was working in the mass data
storage busniess! Loose hardware was the largest reason for product returns.
Dan
----- Original Message -----
From: "Barr, Bob" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, August 07, 2003 9:59 AM
Subject: Re: [TN] marking screws at torque step


> Phil,
>
> A Goggle search turned up the following:
>
> http://www.tohnichi.com/whatsnew4.html
>
> This is neat. Never knew this type of thing existed. We do not mark
hardware
> that has been torqued.
>
> =========================
> Bob Barr
> Manufacturing Engineering
> Formation, Inc.
> =========================
>
> > -----Original Message-----
> > From: Phil Nutting [mailto:[log in to unmask]]
> > Sent: Thursday, August 07, 2003 12:49 PM
> > To: [log in to unmask]
> > Subject: [TN] marking screws at torque step
> >
> >
> > Good afternoon,
> >
> > Does anyone have the requirement to mark hardware that has
> > been set to a specific torque? We currently use an air
> > driven driver and then follow with a paint marking pen. Is
> > there a tool on the market that can torque and mark the
> > hardware in one step? Torque range typically 6 inLb to 50
> > inLb, hardware type either Phillips head or hex head.
> >
> > Thanks in advance.
> >
> > Phil Nutting
> >
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2