Hi do you mean the volume of solder with respect to the volume paste
printed?
Roughly: For Sn63 Sn62 stencil grade pastes, half [50%] the paste volume is
solder. This is good enough most of the time.

Precisely: you can work it out if you know the density of the alloy, density
of the paste flux vehicle and metal percent of the particular paste you are
using. You convert the relative weights (as advised by paste suppliers,
should be written on the jar) to volumes according to the densities.

Example:

Sn63 paste 90% by weight solder.
Density Sn63 = 8.4
Density flux = 1.0 (you should check with your supplier)

So 100 gram of solder paste is 90 gram of metal and 10 gram of flux.

90 grams of metal is (90 / 8.4 =) 10.70 cc
10 grams of flux is (10 / 1.0 =) 10.00 cc

You can do your own percents!

So if you actually do know what volume you have printed you know how much
solder you have per pad.



Regards

Mike Fenner

Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Yannick
Brisson
Sent: Wednesday, August 06, 2003 6:24 PM
To: [log in to unmask]
Subject: [TN] solder fillet


Hi,

  I would like to calculate the solder fillet left on the pad after a
reflow( does it change depending on the component of the pad?), does anyone
know the formula to do that or knows a web site that describ how to do it?

Thank You

Yannick

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2