Hi Werner,
Thanks,
By now I have seen quite a bit of ATC presentations for Lead Free and I am
a bit surprised that this is the first time I have read about a soak or
dwell time at each temperature extreme. Most have reported that they just
go up and then back down in temperature. 30minutes up and 30 minutes down,
thus 24 cycles a day across the range they have selected seems quite common.
Any comments??
Have you also seen this type ATC procedure?
YiEngr, MA/NY DDave
-------------------------------------------------------------------------------Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------