Steve,
To quote" Mountain Dew" Doug;It depends.
There are a lot of things to consider,but the safest choice is Immersion
Silver.
Dewey
> -----Original Message-----
> From: Steve Gregory [SMTP:[log in to unmask]]
> Sent: Thursday, August 28, 2003 9:31 AM
> To: [log in to unmask]
> Subject: [TN] Immersion Silver vs. White Tin
>
> Hi All!
>
> Got a customer that's calling out on the fab drawing, either Immersion
> Silver or White Tin for a board finish.
>
> Me, not having great deal of experience with either one (yet), am
> wondering if I had to choose, which one would I choose?
>
> Have any of you worked with both, and have a preference of one over the
> other? Why?
>
> As always, thanks in advance!
>
> -Steve Gregory-
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|