Howard,
If you peel the tape back and feel sticky adhesive, it's Pressure
Sensitive. If there is no adhesive, it's Heat Sensitive.
Jason
"Howard Watson"
<Howard.Watson@am To: [log in to unmask]
etek.com> cc: "TechNet E-Mail Forum." <[log in to unmask]>
Subject: Re: [TN] SOT 23 placed upside down
07/10/2003 09:32
AM
Jason,
I'm not sure if it is HSA or PSA, how do you tell the difference? With the
feeders we are using (Samsung), it's hard to believe there is enough room
for the component to flip in the pocket as the pocket is well covered where
the cover tape is separated. I'll do a sample to see if any are loaded
upside down. Thanks.
Howard Watson
SMT Manufacturing Engineer
AMETEK/Dixson
Jason.Gregory@l
abarge.com To: "TechNet E-Mail Forum."
<[log in to unmask]>, Howard Watson
<[log in to unmask]>
07/09/03 10:31 cc: [log in to unmask]
AM Subject: Re: [TN] SOT 23 placed upside
down
To help with your first question.....I would do a sample inspection on a
reel to see if the SOT is loaded in the tape upside down. If it is not, it
is flipping during tape pull-back. Are you using HSA or PSA tape? If you
are using PSA, then the adhesive may be mis-registered and grabbing the
part somehow.
For your second question, I would never allow tape and reel for even 50 mil
parts and definitely not 20 or 25 mil.
Jason Gregory
SMT Production Supervisor/
Integrated Product Team Leader
LaBarge Inc.
(918)459-2367
(918)459-2221 fax
[log in to unmask]
http://www.labarge.com
Howard Watson
<Howard.Watson@AM To:
[log in to unmask]
ETEK.COM> cc:
Sent by: TechNet Subject: [TN] SOT 23 placed
upside down
<TechNet@listserv
.ipc.org>
07/09/2003 11:16
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Howard
Watson
Dear Technet folks,
I am obviously not following the search protocol properly for the
information that I need, so I'll just post my Q's anyway. First question
relates to a problem I'm experiencing with some SOT 23's that get placed
upside. This occurs on multiple machines/feeders, and my hunch is that the
component somehow is flipping upside down in the pockets while in the
feeder. Anyone have experience with this problem? I did change the laser
centering parameters so that it gets rejected now if it's upside down, but
I'd like to figure out the root cause.
My second question is regarding QFP components in trays or tape & reel - is
there a standard or recommendation for putting fine pitch QFP's in trays
verses tape & reel? In other words, are 25 or 20 mil pitch gull wing QFP's
OK to be supplied in tape & reel, or should they be in trays to avoid lead
damage? We always get these components in trays, and I figured it was to
protect the leads, but now I wonder if tape & reel is fine. I'm sure it
depends somewhat on the feeders, and their ability to deliver the
components without damaging the leads. Any advice will be greatly
appreciated.
Howard Watson
SMT Manufacturing Engineer
AMETEK/Dixson ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Grand Junction, CO
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|