If you are doing mechanical feasibility, you should use PCB with copper.
The mechanical property would be different with and without copper.
(CTE for example and thermal conductivity for another example...
Stiffness, tensile strength etc.etc.etc.). Better get the real thing.
My 1.38 cents.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>Charles J Wills
>Sent: Tuesday, July 29, 2003 11:02 AM
>To: [log in to unmask]
>Subject: [TN] Scrap PCB Material
>
>
>Does anyone know where I can get some scrap PCB material (FR4 or other,
>0.062") with no copper? I need to make a mock-up of a future
>design to prove the mechanical feasibility of it.
>
>Thanks,
>Charles Wills
>[log in to unmask]
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
>mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|