Hi All,
I am experiencing open solder issue on GSI LQFP (14mmx20mm) package.
The assembly has both GSI and Hynix LQFP package. There is no
problem on Hynix. I use 5-mil laser cut stencil. Reflow temperature
should be OK since Hynix and all the other parts are fine. So I think it might be
coplanarity issue on GSI part. It is in tape and reel.
Do you have the same issue? What is the cause you think? How do you fix it?
Thanks in advance.
Best Regard,
Wei
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------