I think keith Calhoan has an idea, I seem to remember a problem where the
pressure of nitrogen was released suddenly after a few days and it caused
bubbles of nitogen to form in the potting compound we were using, we had to
bake in a presurized oven to force the bubbles to go back into solution.
easy way to test, put some newly mixed compound in a clear container
pressurze and try releasing the pressure after a few days to simulate in use
problem.you might be able to accualy see the bubbles form when the pressure
is released.
Robert tarzwell megadawn.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------