Siggi
An oxygen concentration of 22 to 26 ppm improves wetting and lowers residue.
Contact: Andy Mackie [[log in to unmask]] at Praxair.
Dave Fish
----- Original Message -----
From: "Zweigart, Siegmund" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 02, 2003 10:54 AM
Subject: [TN] Wave soldering / Closed open N- Tunnel systems
> Hello all
>
> We are looking about the differences in lead free wave soldering in regard
> to different wave systems.
> Do somebody know of any experiments regarding different ppm levels if
closed
> (tunnel system) and open N- systems are compared?
> Are ther any differences in Solder Quality in regard to differnt O- levels
> in N?
>
> Thanks for your answers
>
> Siggi
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------