Bill,
I encountered vapor phase in a former life and although I have never used
step soldering, found vapor phase to be unequalled in thermal distribution.
The only downside is cost of media (fluid) and some on this forum have
spoken of possible health and ozone concerns in regards to fluorinated
fluids. We used Galden and 3M fluid and it wasn't cheap. Results were
excellent.
Jason Gregory
SMT Production Supervisor/
Integrated Product Team Leader
LaBarge Inc.
(918)459-2367
(918)459-2221 fax
[log in to unmask]
http://www.labarge.com
[log in to unmask]
Sent by: TechNet To: [log in to unmask]
<TechNet@listserv cc:
.ipc.org> Subject: Re: [TN] Double-sided reflow with Altera RQFP...
07/02/2003 07:19
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
Wgkenyon2
A historical note: What ever happened to step soldering using different
vapor
phase fluids of precise boiling points? As I recall there was a paper on
this
by NT (?) about such a process run very successfully at their West Palm
Beach
facility at one of the NEPCON technical proceedings some years ago.
Proper selection of the alloys used and the K-Fluids (which boiled about 30
degrees apart, as I recall) allowed this step soldering to be done with
ease.
In some cases, mixed K-Fluids were used to 'tailor' the vapor phase to the
alloys in use. The entire range went from K-6 (typical for eutectic
tin-lead) up
to K-10, which could melt pure tin.
Bill Kenyon
Global Centre Consulting
P.O. Box 553, Montchanin, DE 19710 USA
Tel: 302.652.4272 Fax: 302.652.5701 Cell: 302.377.4272
email: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|