TECHNET Archives

July 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="windows-1252"
Sender:
Subject:
From:
Dave Chapman <[log in to unmask]>
Date:
Wed, 9 Jul 2003 12:44:09 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Chapman <[log in to unmask]>
Parts/Attachments:
text/plain (144 lines)
My assumption is that the component code (model) is the same which is why
you are seeing the issue on different machines and feeders. The other
variable is the reel, checking lot code and determining if this has always
been an issue or is new issue are critical to the path for fixing the
problem. We just rejected 6 reels of parts because the parts were sticking
in the paper tape due to excessive adhesive on the paper bottom for a
resistor. It was confined to one lot code and the manufacturer has since
changed the process.

Pick up height, if too large a gap the vacuum will suck the part up from the
reel and it can flip. For SOT23's we have a -.10 mm gap.


For 25 mil we have several parts on tape and reel. Packaging is robust and
we have not seen issues with bent leads. We have run 20 mil TSSOP on the
fine pitch placement machine without problems but I would want lead
recognition for those parts so we changed it back to T&R. I guess a lot will
depend on the quality of the placement equipment.

Dave Chapman
Manufacturing Engineer
Circuit Service Inc.


-----Original Message-----
From: Jason W. Gregory [mailto:[log in to unmask]]
Sent: Wednesday, July 09, 2003 11:31 AM
To: [log in to unmask]
Subject: Re: [TN] SOT 23 placed upside down


To help with your first question.....I would do a sample inspection on a
reel to see if the SOT is loaded in the tape upside down. If it is not, it
is flipping during tape pull-back. Are you using HSA or PSA tape? If you
are using PSA, then the adhesive may be mis-registered and grabbing the
part somehow.

For your second question, I would never allow tape and reel for even 50 mil
parts and definitely not 20 or 25 mil.



Jason Gregory
SMT Production Supervisor/
Integrated Product Team Leader
LaBarge Inc.
(918)459-2367
(918)459-2221 fax
[log in to unmask]
http://www.labarge.com






                      Howard Watson
                      <Howard.Watson@AM        To:
[log in to unmask]
                      ETEK.COM>                cc:
                      Sent by: TechNet         Subject:  [TN] SOT 23 placed
upside down
                      <TechNet@listserv
                      .ipc.org>


                      07/09/2003 11:16
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to Howard
                      Watson







Dear Technet folks,

I am obviously not following the search protocol properly for the
information that I need, so I'll just post my Q's anyway.  First question
relates to a problem I'm experiencing with some SOT 23's that get placed
upside.  This occurs on multiple machines/feeders, and my hunch is that the
component somehow is flipping upside down in the pockets while in the
feeder.  Anyone have experience with this problem?  I did change the laser
centering parameters so that it gets rejected now if it's upside down, but
I'd like to figure out the root cause.

My second question is regarding QFP components in trays or tape & reel - is
there a standard or recommendation for putting fine pitch QFP's in trays
verses tape & reel?  In other words, are 25 or 20 mil pitch gull wing QFP's
OK to be supplied in tape & reel, or should they be in trays to avoid lead
damage?  We always get these components in trays, and I figured it was to
protect the leads, but now I wonder if tape & reel is fine.  I'm sure it
depends somewhat on the feeders, and their ability to deliver the
components without damaging the leads.  Any advice will be greatly
appreciated.

Howard Watson
SMT Manufacturing Engineer
AMETEK/Dixson ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

Grand Junction, CO

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2