Thank you to all.
We have a BGA package that we suspect for Pop corning or
delaminating that we need to have scanned.
As usual, Tech-Net comes thru with sound advice and help.
My hat is off to the Net.
You too Duane......
Barry.
-----Original Message-----
From: Collins Graham [mailto:[log in to unmask]]
Sent: Wednesday, July 30, 2003 1:22 PM
To: [log in to unmask]
Subject: Re: [TN] SAM Microscope
Hi Barry
As another Technetter indicated, SonoScan is the big company making
these things. They will happily sell you one, or if you just need some
small jobs done they do work on analysis by contract. They will provide
a full report with analysis, pretty thorough - and color pictures to
impress the boss.
Good equipment to look for die delamination within a chip, and we've
used them to check for voiding in underfill materials. We also used
them to check for package delamination on some ICs where we had to
re-form the leads a bit...
I believe they have offices in California and in near Chicago.
http://www.sonoscan.com/
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
>>> [log in to unmask] 07/30/03 03:33PM >>>
I have just had a discussion with a fellow associate,
and he is on the hunt for somebody able to do
something called SAM (Scanning Acoustic Microscope.)
Anyone heard of any such animal.
Barry
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|