TECHNET Archives

July 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Frank L Norman <[log in to unmask]>
Date:
Tue, 29 Jul 2003 09:43:58 -0700
MIME-Version:
1.0
X-To:
"Kasprzak, Bill (sys) USX" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Frank L Norman <[log in to unmask]>
Parts/Attachments:
text/plain (82 lines)
Bill,

Solder wetting can not be achieved to these plated through holes by hand
touched-up, including the use of RMA flux or Soldernew(machanical
abrasion). Note, water soluble flux(Alpha Metals WS362-25)was originally
used in the wave solder fluxing process.

Regards,
Frank Norman
Manufacturing Support Engineer
Raytheon, Space and Airborne Systems (SAS)
(805)879-2745
[log in to unmask]





"Kasprzak, Bill (sys) USX" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/29/03 08:38 AM
Please respond to "TechNet E-Mail Forum."; Please respond to "Kasprzak,
Bill (sys) USX"


        To:     [log in to unmask]
        cc:
        Subject:        [TN] Lead Junction Temperature


Hello all,

Is there any data or study that I can use that shows what the internal
junction temperature of a leaded device is when removing a part with a
solder sucking operation. Is there any reason why an IC, diode, or cap
cannot be re-used when removed from a circuit board prior to test if the
device was installed with incorrect polarity? I think that the PWB serves
as
a buffer when desoldering from the solder side and therefore the part is
protected.

We are in the launch vehicle business. There are some that say a part can
only be soldered once. So, a diode soldered into a board cannot be removed
and re-soldered correctly even though no power has been applied. The
unsoldered part must be discarded and replaced with a new part.

Any ideas how this relates to surface mount?

I know that part re-use takes place all the time but the fact that launch
vehicles are involved fosters a very conservative approach. Any comments
from the high-rel, class 3 folks?

Thanks to all who can respond, I really appreciate it.

Bill Kasprzak
Moog Inc, Electronics Process Engineering

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2