Hi Douglas,
I never profile in "wet" paste.
For "high rel" electronics we also have to scrap a board, using almost the
same method as you do.
But for standard applications I only have to scrap a new bare board.
I use old scrapped components to populate the board, creating the same
circumstances as with the real board.
But the thermocouples are never placed in wet paste.
What is the benefit of doing that?
Is the profile that different if I attach the thermocouple on a solid
solderjoint?
Jowan Iven
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McCall,Doug
Sent: dinsdag 29 juli 2003 9:34
To: [log in to unmask]
Subject: [TN] Attaching mole thermocouples to PCBA's being profiled at
reflow
Hi all,
When profiling a PCB assembly through a reflow oven process
how do you guys actually attach the thermocouples. The reason
for asking this question is that if you attempt to put the wires
(x6) over the wet solder paste then the components & devices will
be moved by the loose thermocouple wires.
Therefore, I have been using a scrap PCB assembly and profiling a
number of times, but this means having a scrap one out of the batch.
Any thoughts appreciated.
Thanks,
Douglas I McCall,
PCB Manufacturing Engineer
BOC EDWARDS,
Marshall Road,
Eastbourne,
East Sussex,
BN22 9BA UK
Tel: +44 (0) 1323 501 147
Fax: +44 (0) 1323 509 824
mailto:[log in to unmask]
_____________________________________________________________________
This e-mail has been scanned for viruses by MCI's Internet Managed Scanning
Services - powered by MessageLabs. For further information visit
http://www.mci.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|