Doug,
Thanks for the response. I hope to be looking into this in the near future. Always searching for better/quicker means of increasing mold compound adhesion, but am not to thrilled with the 3DT approach of blowing an arc across all of my little antennae (wire bonds).
Yours was the only response off both forums.
In addition to yours, here are a few others that I hope to follow through on.
Steven Creswick
Materials and Process Leader
Gentex Corporation
Zeeland, MI
http://www.hanmico.com/project/others_plasma.htm
http://www.surfxtechnologies.com/default.htmSurfx
http://3dtllc.com/
http://www.corotec.com/
http://www.pillartech.com/corona_tech.html
http://www.sigmalabs.com/sigma/atmosplas.htm
http://www.enerconind.com/treating/
http://www.rycobel.be/Voorbehandelinge.htm
http://plasmasystems.com/core.html
-----Original Message-----
From: Doug Pauls [mailto:[log in to unmask]]
Sent: Thursday, June 05, 2003 12:07 PM
To: [log in to unmask]
Subject: Re: [TN] Experience with Atmospheric Pressure Plasma Cleaners
Steve,
A few months ago we had one of our vendor reps come through. He gave me
some flyers on an offering from Tri-Star Technologies. The model was
PT-2000. Tri-Star is in El Segundo, California. Phone 310-536-0444.
www.tri-star-technologies.com. I have not gotten around to looking at this
in any depth.
Doug Pauls
"Creswick,
Steven" To: [log in to unmask]
<SCreswick@GENTEX cc:
.COM> Subject: [TN] Experience with Atmospheric Pressure Plasma Cleaners
Sent by: TechNet
<TechNet@listserv
.ipc.org>
06/05/2003 10:12
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Creswick,
Steven"
Dear All,
Forgive me (somewhat) for cross-posting this to both Chip and TechNet
forums, but I am curious if anyone out there has had experience with the
new(er) atmospheric pressure plasma cleaning systems that are beginning to
pop up.
This is specifically aimed at the FC, COB, COG, or Hybrid people out there.
A couple atmospheric pressure plasma equipment manufacturers include:
Surfx Technologies and Han-Mi
So, has anyone heard of, played with, used, or tried any??
Please share what you can.
Steven Creswick -
Gentex Corporation
600 North Centennial St
Zeeland, MI 49464
Ph 616 772 1590
Fx 616 772 2690
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|