In addition to the great list Carrie provided, you may want to consider the
following:
* Ease of removal for various features and configurations of
application
* Resistance to breakdown in the flux and solderwave
* Ionic characteristics of the mask
* Compatibility with board and final finish materials
* Applied shelf life
* dispensable Vs screenable
If you are post wavesolder washing the boards have you considered a soluble
mask instead of peelable which can be difficult and time consuming to
remove?
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Tenison Stone [mailto:[log in to unmask]]
Sent: Thursday, June 12, 2003 12:10 PM
To: [log in to unmask]
Subject: [TN] evaluation of peelable solder mask for wave solder
Hi everyone,
I am working on a plan to evaluate peelable solder masks for wave soldering.
We currently use a latex that takes overnight to dry. I have several
samples from different vendors to use in an experiment.
What parameters should be included in the experiment to ensure I make the
best decision for my process?
Thank you for your help.
Tenison Stone
Manufacturing Engineer
Telex Communications
1930 West First Street
Blue Earth, MN 56013
507-526-3205 x2164
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
507-526-3059 (fax)
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|