James,
I'd go back to my board fab company and tell them to clean their immersion silver plating line. If you are seeing silver pull off the board that usually means the chemistry isn't in control and the rollers in the plating line have silver plated on them and when they toudh the board surface they transfer small pieces of silver to the board. These small pieces are not plated on the board but "lightly stuck" (i.e., they will pull off if you do a tape test.
Regards,
George
George M. Wenger (908)-546-4531
Reliability Engineer
RF Power Amplifier Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: Cagle, James [mailto:[log in to unmask]]
Sent: Tuesday, June 17, 2003 10:21 AM
To: [log in to unmask]
Subject: [TN] Emersion Silver
We are currently building boards with emersion silver. I have 2 questions.
1: We have 2 boards where the plating has come off (small 1/8" diameter
circle) and on some mounting holes on the other. What are some of the ways
to repair it?
2: We are using kapton tape to protect silver ground plane in the SMT
process from solder balls?
Is this the norm or is there a better way?
James Cagle
Tyco
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|