You guys are scaring me now, see if you had told me about all these problems
I would of never been out in the plating shop fabricating these selective
gold boards for the past 20 years! But now that I know all this scary stuff
about differential galvanic etching, resist breakdown, added cost,
dissimilar metal interface problems, etc, etc I must have been crazy or
dreaming thinking we could do that; but we did. We now also have various
outside suppliers doing the same processes.
Sure it's not easy. It took a lot of development work and effort. You must
control your plating bath chemistry, carbon treat cycles, make sure your
anodes and plating racks are maintained, establish the right current
densities, use the correct plating resist. Etcher variables must be closely
controlled, chemistry, temperature, conveyor speed, operator awareness.
Circuit design that has the proper feature sizes, interfaces, plating
robbers.
Most of this is based in science but there also a bit of black magic in
there that you can't buy from an equipment or chemical supplier at any
price. Unless you thoroughly see and understand the big picture anyone of
these and more will bite you, as you probably know.
Too often we are told things are impossible or too difficult to do. It's
easy to say we can't do that. That's when the guy next door will figure out
how to do it and will eat your lunch.
Dougal, By the way our customers do not pay extra for our equipment. The
cost of the selective gold plate which is used on our rotary switch products
creates a more robust contact area than say ENIG. This allows us to use a
much more simpler and inexpensive rotary switch design which gives a lower
overall cost to the product and still provide a lifetime warranty.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Dougal Stewart [mailto:[log in to unmask]]
Sent: Tuesday, June 24, 2003 2:37 PM
To: TechNet E-Mail Forum.; Barmuta, Mike
Subject: Re: [TN] (2) [TN] Electro-Plated Ni/Pd/Au vs [ENIG]
Mike, I'm glad you have a supplier willing to do selective electroplate for
anything other than gold edge contacts, and I'm happy that you have
customers who are willing to pay the extra for your equipment because of
more expensively processed bare boards. Yes, it is possible to do selective
electroplate of features, but it adds to the processing (more lamination and
print steps), increases the risk of failure (etching problems due to
different metal electron levels), and is NOT designed for manufacture. I
used to make a very large complex 26 layer board with 3 mil buried cores, 4
mil line and space everywhere, 6 mil holes, laser vias 1 - 3, ZBC layers,
and multiple impedances on many layers, yet the thing that blew our yields
was the selective electroplated nickel gold areas for LGA components.
Dougal Stewart
email: [log in to unmask]
phone: +44 1896 822204
mob: +44 7984 629667
www.pwbsolutions.co.uk
----- Original Message -----
From: "Barmuta, Mike" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, June 24, 2003 9:23 PM
Subject: Re: [TN] (2) [TN] Electro-Plated Ni/Pd/Au vs [ENIG]
> Hi Chris: Sorry but I have to disagree with you regarding hard gold "
> requiring the ENTIRE board be plated with gold". It does not require the
> complete outerlayer circuitry to be plated with gold.
> Selective electroplated hard gold is fairly common. It can be done either
> before or after copper pattern plate. The rest of the exposed copper
> pattern plate circuitry use whatever the normal etch resist plating is,
> typically tin. The key is in how you design the plating resist layers and
> the interface between then gold and copper features.
>
> Then of course there is bussed gold plate usually done with gold
> tips/fingers.
>
> We build several thousand boards a week thru our PCA processes using
> selective hard gold.
>
>
> Just out of curiosity why are you removing the gold from your surface
mount
> pads? Is it too thick for reliable solder joints due to a thickness
> requirement you have? If so you can actually do a double gold where SM
pads
> get one thickness and other features have a heavier deposit for things
like
> rotary switches.
>
>
> Regards
>
> Michael Barmuta
>
> Staff Engineer
>
> Fluke Corp.
>
> Everett WA
>
> 425-446-6076
>
>
>
> -----Original Message-----
> From: Chris Robertson [mailto:[log in to unmask]]
> Sent: Tuesday, June 24, 2003 12:36 PM
> To: [log in to unmask]
> Subject: Re: [TN] Electro-Plated Ni/Pd/Au vs [ENIG]
>
>
> Scott,
> There a few versions of the gold plating. Hard gold requires the ENTIRE
> board be plated with gold. Some are reportedly capable of doing this
> selectively, but since the gold is used as an etch resist, it really is
> difficult.
>
> The problem we encounter is we must remove the gold from all surface mount
> pads (not through hole) before soldering. A very time consuming process.
I'm
> not familiar with the ENIG (or I just don't recognize it)
> I'm not sure what palladium get you in the mix.
> Gold is a great antioxidizing metal (what it is used for in this case) and
> has a long shelf life unlike entek and some other coatings. The nickel is
> for hardness. If you do use/change to this, ask the forum about the mix.
> There are some common ratios for nickel/gold. I personally don't have one
> that includes Pd.
>
> Chris Robertson
> Design Engineer
> Lockheed-Martin Technology Services
> 4912 Research Dr.
> Huntsville, AL 35805
> (256) 722-2626
> [log in to unmask] <mailto:[log in to unmask]>
>
>
> I have a new board shop promoting their Electro-Plated Ni/Pd/Au (hard or
> soft gold) surface finish over our existing [ENIG] boards. We have not
had
> any issues with our current assemblies using [ENIG]. I am requesting any
> advice or information on Electro-Plated Ni/Pd/Au and if it would be worth
> switching to it. Any advice would be greatly appreciated, thank you in
> advance.
>
>
>
> SCOTT
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|