In addition to Mike's additions to Carrie's great list, you need to
consider the effects of outgas products on nearby metals. Some of the
latex material outgas ammonia, acetic acid, or alchols. These can and do
get into other components and can tarnish metals, especially if working
with silver.
Doug Pauls
Rockwell Collins
"Barmuta, Mike"
<Mike.Barmuta@FLU To: [log in to unmask]
KE.COM> cc:
Sent by: TechNet Subject: Re: [TN] evaluation of peelable solder mask for wave solder
<TechNet@listserv
.ipc.org>
06/12/2003 03:39
PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Barmuta, Mike"
In addition to the great list Carrie provided, you may want to consider
the
following:
* Ease of removal for various features and configurations of
application
* Resistance to breakdown in the flux and solderwave
* Ionic characteristics of the mask
* Compatibility with board and final finish materials
* Applied shelf life
* dispensable Vs screenable
If you are post wavesolder washing the boards have you considered a soluble
mask instead of peelable which can be difficult and time consuming to
remove?
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Tenison Stone [mailto:[log in to unmask]]
Sent: Thursday, June 12, 2003 12:10 PM
To: [log in to unmask]
Subject: [TN] evaluation of peelable solder mask for wave solder
Hi everyone,
I am working on a plan to evaluate peelable solder masks for wave
soldering.
We currently use a latex that takes overnight to dry. I have several
samples from different vendors to use in an experiment.
What parameters should be included in the experiment to ensure I make the
best decision for my process?
Thank you for your help.
Tenison Stone
Manufacturing Engineer
Telex Communications
1930 West First Street
Blue Earth, MN 56013
507-526-3205 x2164
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
507-526-3059 (fax)
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|