Copper density = .31 lbs / Cubic inch
1 lbs / Cubic inch = 27648 oz /Cubic Foot
Copper density (.31 * 27648) = 8570 oz / Cubic foot
2 oz Copper cubic foot
----------- X ---------------- = .000233 foot
Square foot 8570 oz copper
.000233 foot x 12 in/ft = .0028 inch
2 oz/ft2 is a weight per area. Divide by a weight per volume (density) and
you get length, or thickness.
What did I miss, other than the metric unit conversions? I admit, I did
miss Paul's first message.
George Franck
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Thursday, June 05, 2003 2:11 AM
To: [log in to unmask]
Subject: Re: [TN] (2) Micro-inch to copper weight conversion..Error
Alert
Hi Paul,
All of this is nice, but.......oz./ft2 is NOT a thickness--it is a weight.
It
does not convert to a fixed thickness value in any of the units you list.
Sorry,
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|