TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Poh Kong Hui <[log in to unmask]>
Date:
Wed, 4 Jun 2003 07:38:48 +0800
Content-Type:
text/plain; charset="us-ascii"
X-To:
"Dobbs, Marie" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Poh Kong Hui <[log in to unmask]>
Parts/Attachments:
text/plain (95 lines)
Hi Technetters,

In fact, which location also dictates the pricing as well other than
volume, in US, Singapore, Indonesia or China.

And also the logistic issue and the total BOM cost.

I was once faced with this issue. The French wants everything in SMT, we
want certain portion of the board in TH. We looked at the BOM cost and
assembly cost, it was more economical for us, but not for the French. And
we had a long debate over this till we settle with our customer where they
want to produce. And that dictates how the board should be designed. And of
course, if you have the space on the board, do incorporate the potential
difficult to find component both in SMT and TH.

Hope that helps.

Poh



At 01:09 PM 5/23/03 -0400, Dobbs, Marie wrote:
>Volume Volume and Volume usually dictate SMT VS TH.
>If you volume is great enough than SMT is the way to go even if you need to
>Loose load a couple of components at hand assembly.  I am not sure which
>tech bulletin or procedure would point you in this direction, but that is
>how business is done here at Tyco.
>Regards
>Marie
>
>-----Original Message-----
>From: Tempea, Ioan [mailto:[log in to unmask]]
>Sent: Friday, May 23, 2003 12:34 PM
>To: [log in to unmask]
>Subject: [TN] Through-hole design vs. SMT design
>
>
>Hi Technos,
>
>I have a dilemma on my hands. An assembly that has about 15 passives (caps
>and resistors), a connector and a fuse holder. The connector must be TH and
>probably so does the fuse holder. The designers came with the question: "for
>lower manufacturing costs should we design the board 100% TH, or make the
>passives SMT and keep the other 2 parts TH". Interesting...
>
>And here come my questions:
>
>*       what are the technical criteria that you use when trying to solve
>this kind of riddle?
>*       what are the economical criteria?
>*       what parameters could I use for a breakeven analysis?
>
>Thank you,
>Ioan
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2