Dear Mike:
Some of the confusion with exposed copper on land areas is derived from
IPC-A-610C at paragraph 6.5.6 Nonwetting. Figure 6.51 shows such a board
with a likely OSP coating board with soldered a "J" lead SMT component.
This is one of the sections I point out that the text take precedence
over the figure (and in this case rightly so).
As for actual experience with OSP PCB's I will leave that to the other
experts.
Gregg A. Owens
Executive Director
Manufacturing Technology Training Center, Inc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of No Name
Sent: Wednesday, June 11, 2003 4:29 AM
To: [log in to unmask]
Subject: [TN] OSP Boards for IPC Class 3 product.
Does anyone out there have experience with OSP and IPC class 3 products?
We have considered changing over to OSP as things shift to lead free. We
also see a cost savings in converting. However, some of our quality
people
do not believe the exposed copper on the edges of the pads is
acceptable. I
see nothing in the J-STD-001 or IPC-610 that says the fillet must cover
the
entire pad. Can anyone relate their experience selling OSP assemblies to
the
military?
Thanks for your replies.
-Mike McGee
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|