TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Franklin D Asbell <[log in to unmask]>
Date:
Wed, 11 Jun 2003 09:05:40 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<009101c33018$351df550$0600a8c0@franklin>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (37 lines)
IPC-A-610C Section 6.5.2 Exposed Basis Metal
SMT ICs, OSP coated PWBs, leaded components, sides of land patterns,
conductors, and use of LPI solder resist, can have exposed basis metal
per original designs.

Note: PWA with alternative finishes (OSP) may exhibit solder wetting
only to specific areas where solder is intended. Exposed metal in
unsoldered areas should be considered normal under these circumstances,
provided the achieved wetting characteristics of the intended solder
connection areas are acceptable.

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of
> Franklin D Asbell
> Sent: Wednesday, June 11, 2003 8:52 AM
> To: [log in to unmask]
> Subject: Re: [TN] OSP Boards for IPC Class 3 product.
>
>
> Mike,
>
> I know a certain amount of exposed copper is allowable on
> bare boards, even for military product. For the bare board we
> reference IPC 6012. Is there an IPC performance standard for
> assembled product?

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2