Why # 1, why would you not want to test with the flux you are using on your
production?
Iain.
-----Original Message-----
From: Munie, Gregory [mailto:[log in to unmask]]
Sent: 08 May 2003 15:11
To: [log in to unmask]
Subject: Re: [TN] Wetting Balance Testing
*** WARNING ***
This mail has originated outside your organization,
either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
Neil
I've done a lot of wetting balance but I have to add a few comments on the
"dip and look." (I agree with all Bev's other comments and suggestions.)
The dip and look as it's traditionally done does deserve to die. But if done
correctly it can tell you almost as much as wetting balance.
And I define correctly as:
1) Use ONLY water white rosin flux. NEVER use any activators in the flux.
2) Control your immersion (wetting balance is good for this :-)
3) Coverage criteria means nothing if you don't see active wetting, i.e.
solder rises ABOVE the surface of the bath to wick UP the part lead.
# 3 is absolutely critical: in a real world soldering situation that is
exactly what you want to happen for either wave or reflow soldering. It's
what happens to the section of the lead that's NOT in direct contact with
the solder that tells you whether the part is solderable.
Greg Munie
Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, May 08, 2003 4:25 AM
To: [log in to unmask]
Subject: Re: [TN] Wetting Balance Testing
Neil,
You also need to consider what alloy you are using. Dr. Lee of Indium has
shown that 62/36/2 Sn/Pb/Ag gives significantly different results. And then
there is the work Chris Hunt et al of the British NPL have done on lead free
solders. And then are you using a solder globule or solder bath? Don't
forget temperature, atmosphere (most likely air, unless like Chris you can
afford a dry box) and preheat (or is that what you mean by hang time?). If
you are using a globule block we have also found that how centered your
component lead is over the solder globule affects your results as well.
I would say it is not so much the length of the lead (unless you are talking
about something obscenely long - no comments please), but rather what the
lead is connected to - like an internal heat sink. And, yes, we have had
ONE problem with the heat sinking ability of a component affecting the
results. I gave a short presentation to the J-STD-002 committee at APEX. I
will send you a copy. It will not show up for other TechNetters,
unfortunately. In essence, we found that wrapping the wetting balance clip
in polyimide tape allowed the component in question to pass solderability
testing!
All said, we have had excellent results using a wetting balance and much
prefer it to the dinosaur "dip and look" test, which I would like to see DIE
for SMT components. Now if we can just agree on what pass/fail criteria
will be....
regards,
Bev Christian
Research in Motion
-----Original Message-----
From: Neil Flatter [mailto:[log in to unmask]]
Sent: May 8, 2003 1:17 AM
To: [log in to unmask]
Subject: [TN] Wetting Balance Testing
For those of you doing solderability testing, what sorts of parameters
should we be concerned about for reliable results? Our tester already
allows inputs for lead perimeter, cross sectional area, and hang time. My
company's testing also specifies immersion angle, depth, and speed as well
as the type of flux. By controlling these factors, can I expect repeatable
results?
It has been suggested that we also need to limit the length of the leads for
our testing as wall as installing a thermal break between the lead and the
hanger. Both have been blamed for failing test results. Has anyone
experienced changes in test results from these variables?
Neil Flatter
TRW-Automotive
Process Quality
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|