The passivation test you describe is pretty standard, and should be a good
test.
Passivation does not change the appearance of the metal, if passivation is
all that is being done, however, some metal treatments do more, and may well
polish as well as passivate, in which case the surface will be
shiney....unless....
The Stainless has a high carbon content, in which case the carbon will not be
dissolved by the polish, and will remain on the surface as a black smut......
which can be removed by a 45 second dip in 50% by volume concentrated Nitric
Acid, preferably in deionized water.
Rudy Sedlak
RD Chemical Company
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|