As we have to go from Gigaver to another solution we are discussing about
Cu- adhesion for this material.
We are thinking of:
Megtron 5, Polycald LD616/LD621; Isola IS620; Neelco 4000 Series.
Are there any practical informations about Cu- Adhesion after soldering. If
I look to the data sheets the values are smaller as Gigaver.
Has anybody measured adhesion values on a real product?
Siggi
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------