TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 22 May 2003 08:32:01 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Content-Type:
text/plain; charset="iso-8859-1"
In-Reply-To:
Organization:
EXFO-TO
MIME-Version:
1.0
Parts/Attachments:
text/plain (128 lines)
You would need good dynamic range (more important than the few thousand
X) to take care of build in heat sink, shielding layer etc. etc.  More
of a problem soon... If it is not now...;-(

jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>Reuven ROKAH
>Sent: Thursday, May 22, 2003 12:43 AM
>To: [log in to unmask]
>Subject: Re: [TN] X-Ray Inspection of BGAs
>
>
>To find shorts - its easy , from the top.
>To find opens - you need to tilt the PCB as much as it
>possible or 3D X Ray. To find voids - you need software to
>measure and calculate the % comparing to IPC , 1 mil accuracy in OK.
>
>Best  Regards
>
>ROKAH Reuven
>
>e mail: [log in to unmask]
>
>
>
>                      "Anderson, Greg
>                      (IndSys,                 To:
>[log in to unmask]
>                      GEFanuc, NA)"            cc:
>                      <Greg.Anderson@G         Subject: [TN]
>X-Ray Inspection of BGAs
>                      EFANUC.COM>
>                      Sent by: TechNet
>                      <TechNet@LISTSER
>                      V.IPC.ORG>
>
>
>                      21/05/03 11:58
>                      PM
>                      Please respond
>                      to "TechNet
>                      E-Mail Forum.";
>                      Please respond
>                      to "Anderson,
>                      Greg (IndSys,
>                      GEFanuc, NA)"
>
>
>
>
>
>Technetters,
>
>We are currently evaluating off-line X-Ray inspection machines
>for the process development and periodic process monitoring of
>BGA, u-BGA, etc Printed Wiring Assemblies.  For those of you
>who have such machines:
>
>1) How important is a feature that allows actual measurement
>of the ball diameter vs. "uniformity" of the balls?  The
>candidate systems accuracy claims vary from +/- 0.001" down to
>+/-0.00025".  Is it possible or desirable to measure and log
>the diameters? (intuitively, I believe so, but maybe the
>"noise" of part to part, or PWA warpage makes this irrelevant).
>
>2)  How important is the ability to view at oblique angles
>greater than 45 degrees?  Do you need to go to 75 degrees?
>
>3)  How much magnification is "enough"?  600X ?  1200X?
>
>4)  Are you able to develop and use "Printed Wiring Assembly
>Specific" programs?  That is, can you build an inspection
>routine to look at one or more locations on the assembly,
>store it, then call it later when that product comes around
>again?  How difficult is it to program?  Can it be done by
>someone other than an engineer?
>
>Please, if you are going to mention specific systems, respond
>off line (and off the record, if need be), to avoid flaming
>repercussions.  I need frank responses.
>
>Thanks,
>Greg Anderson
>Senior Mfg Engineer
>GE Fanuc Automation
>phone:  434-978-5181
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2