George
With an unstabilised and unbuffered solvent and fine aluminium powder,
the reaction with some halocarbons may be sufficiently rapid and
exothermic to be considered as explosive. Obviously, at the temperatures
involved, hydrogen halides and carbonyl halides (such as phosgene) may
be formed as breakdown products. This could be dangerous but very
unlikely to happen in real life, although superficial attack of
amphoteric metal and alloy surfaces is not unknown with badly maintained
solvents.
Brian
Carroll, George wrote:
> What were the conditions? How violent is the reaction? Explosive or just
> corrosive? Finely divided metals tend to be much more reactive than sheet
> metal. If there were a bit of humidity, especially at an elevated
> temperature, might there not be a bit of HCl liberating hydrolysis taking
> place?
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|