Based on my copy of MIL-STD 2000 (remember that one), Section 4.18.3:
MIL-P-28809 - Beckman: 10.06 ug NaCl / sq. in.
MIL-P-28809 - Markson: 10.06 ug NaCl / sq. in.
Omegameter: 14 ug NaCl / sq. in.
Ionograph: 20 ug NaCl / sq. in.
Ion Chaser: 32 ug NaCl / sq. in.
Hope this helps.
Good Luck
Lee Whiteman
Senior Manufacturing Engineer
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x208
Fax: (610) 362-1290
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Poh Kong Hui
Sent: Thursday, May 01, 2003 12:21 PM
To: [log in to unmask]
Subject: [TN] : Ionic contamination limit level for Ionograph
Hi All,
I would like to know what is the limit level for board cleanliness, if
using Ionograph. I remember the limit level for using Omegameter is 14,
but can't remember what unit.
Please enlighten me.
Thanks.
Poh
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|