I thought I qualified my analysis in the last statement:
"Of course, the copper used is probably not the pure Cu which has a density of 8.2 g/cm3, so that actual thickness may be off somewhat from this calculation."
Guess that wasn't specific enough.
Happy Friday!
>>> [log in to unmask] 05/30/03 03:49PM >>>
Hi Blair,
Unfortunately, your assumption that you know the specific gravity (density)
of ED copper is incorrect--you do not know it--it is less than the specific
gravity (density) of rolled copper because of organic co-deposits and
micro-voids. This uncertainty in specific gravity (density) prevents a direct conversion
of oz./ft2 to thickness, and thhat is why ED copper is spec'd in oz./ft2.
Regards,
Werner Engelmaier
Fornercahairman of IPC Copper Fopil Committee
**********************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|