TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brian Ellis <[log in to unmask]>
Date:
Fri, 30 May 2003 13:46:11 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Content-Type:
text/plain; charset="iso-8859-1"
In-Reply-To:
Organization:
EXFO-TO
MIME-Version:
1.0
Parts/Attachments:
text/plain (109 lines)
http://www.johnsonmfg.com/temp/J35TX.htm
Never use this before... But did use some acid flux....(can't find it
anymore).
                                                              jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>Brian Ellis
>Sent: Friday, May 30, 2003 2:59 AM
>To: [log in to unmask]
>Subject: Re: [TN] Nickel plated wire...
>
>
>Steve
>
>I agree with David and, in fact, would NOT recommend
>Ni-plating for soldering to. It can be reliably soldered using
>strong halide-activated fluxes, preferably water-soluble. You
>may not wish to use these for rework for obvious reasons. As
>David says, pretinning is a good solution provided you wash
>off the flux residues from the pretinned wire. But then,
>pre-tinned wire is no longer nickel plated, is it? It is
>tinned. So why not use tinned wire in the first place? This is
>obvious and I cannot understand a MIL spec that disallows
>tinned wire and allows silvered wire, which could whisker like
>hell if you so much as curve it into place. Doesn't make
>sense. But then neither do thousands of specs, standards and
>other regulations written by technocrats whose only aim in
>life is to ensure they appear busy enough to keep their cushy
>job. I have always claimed that good commonsense, based on
>science, is worth more than ten-thousand standards. This is
>just a case in point.
>
>Brian
>
>Steve Gregory wrote:
>> Hi All,
>>
>> I was posed this question by one of our customers. I don't have any
>> experience with nickel plated wire, but it would seem to me to be
>> difficult to solder to. I've used tin plated, and silver plated wire
>> before with no problems. But I didn't know that silver
>plated wire had
>> corrosion problems. Any inputs?
>>
>> In the future we are going to be changing to specify a nickel plated
>> wire (M22759/10-28-9) for PWA repair.  The previous part
>number was a
>> silver plated wire.  We haven't used this before.  Do you or any of
>> your manufacturing people know of issues with solderabiliby
>when using
>> a nickel plated wire or any special process that should be used?
>>
>> The history of this is IPC-7721 paragraph 6.1 says silver
>plated wire
>> must not be used because it can cause corrosion of wire in certain
>> situations. Turns out that when you follow MIL-23200 the
>allowed wire
>> is either silver plated or nickel plated.  We would have
>preferred tin
>> plated wire but it doesn't appear to fall under the allowed
>MIL-23200
>> options.
>>
>> Thanks in advance!!!
>>
>> -Steve Gregory-
>> ---------------------------------------------------
>> Technet Mail List provided as a free service by IPC using LISTSERV
>> 1.8e To unsubscribe, send a message to [log in to unmask] with
>following
>> text in the BODY (NOT the subject field): SIGNOFF Technet To
>> temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/html/forum.htm for additional information, or
>> contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>> -----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
>mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2