TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Zweigart, Siegmund" <[log in to unmask]>
Date:
Fri, 30 May 2003 10:01:06 +0200
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Zweigart, Siegmund" <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
-----Original Message-----
From: Zweigart, Siegmund
Sent: Mittwoch, 28. Mai 2003 18:23
To: 'TechNet E-Mail Forum.'
Subject: Cu- adhesion on HF- Materials


Hello to all

As we have to go from Gigaver to another solution we are discussing about
Cu- adhesion for this material.
We are thinking of:
Megtron 5, Polycald LD616/LD621; Isola IS620; Neelco 4000 Series.
Are there any practical informations about Cu- Adhesion after soldering. If
I look to the data sheets the values are smaller as Gigaver.
Has anybody measured adhesion values on a real product?

Siggi

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2