hi,
i think, but am not certain, that i understand your question.
first of all, i interpret nickel/tin plating to be 'pure' nickel with 'pure' tin deposited on top of it. if this is the case, you haven't gotten rid of the magnetic nickel.
second, nickel-only is not a good finish to solder to to say the least
third, specifically, what do you mean by reliability?
phil
-----Original Message-----
From: Stolar, Paul W [mailto:[log in to unmask]]
Sent: Wednesday, May 21, 2003 1:33 PM
To: [log in to unmask]
Subject: [TN] PCB plating
Does anyone have any knowledge about Ni versus Ni/Sn plating as it
relates to reliability? We cannot use pure Ni since it is magnetic.
Any ideas about how thicker Pd will affect reliability?
Paul Stolar
Materials Engineer
Houston Technology Center
Baker Atlas
713-625-5376
713-625-4949 (fax)
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|